Carbon Fiber-Reinforced Polymer for Continuity in Existing Reinforced Concrete Buildings Vulnerable to Collapse

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Carbon Fiber-Reinforced Polymer for Continuity in Existing Reinforced Concrete Buildings Vulnerable to Collapse

Author(s): Sarah Orton, James O. Jirsa, and Oguzhan Bayrak

Publication: Structural Journal

Volume: 106

Issue: 5

Appears on pages(s): 608-616

Keywords: carbon fiber-reinforced polymer; catenary action; continuity; progressive collapse; structural integrity

DOI: 10.14359/51663101

Date: 9/1/2009

Abstract:
Carbon fiber-reinforced polymer (CFRP) can provide continuity in reinforced concrete beams and thereby reduce the likelihood of progressive collapse if a supporting column were lost due to extreme loading (blast or impact). Seven half-scale specimens representing two spans of a reinforced concrete (RC) frame with a center supporting column removed were tested. The capacity of vulnerable RC building beams with discontinuous reinforcing steel were evaluated and compared with beams using CFRP to provide continuity, and with beams designed with continuous reinforcing steel. It was found that CFRP is capable of providing sufficient continuity to withstand the loss of a supporting column through either catenary (or cable) action, which reduces material usage, or flexural action, which reduces deflections. Furthermore, beams with continuous reinforcement may not be able to withstand the loss of a center-supporting column due to limited rotational ductility of the beam.