Title: 330.1-94: Standard Specifications for Plain Concrete Parking Lots

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 7

Keywords: parking lots

DOI:

Date: 1/1/1994

Abstract:

Note: A newer version of this document exists. This document was replaced by 330.1-03.

This standard covers minimum requirements for the construction of plain concrete parking lots on grade. Included are requirements for materials, placing, texturing, curing, jointing, and opening to traffic.