Title: Designs of Concrete Bridges with Multiple Box Cells Due to Torsion Using Softened Truss Model

Author(s): Chung C. Fu and Daili Yang

Publication: Structural Journal

Volume: 93

Issue: 6

Appears on pages(s): 696-702

Keywords: bridge design; multiple box; reinforced concrete; torsion; softened truss model;

DOI: 10.14359/516

Date: 11/1/1996

Abstract:
Using a softened truss model, this paper presents a method for torsional design of multicell concrete bridges. Earlier researchers have successfully shown the development for solving single cell torsion by combining the equilibrium, compatibility, and the softened constitutive laws of concrete. By solving the simultaneous equations based on the membrane analogy, multicontinuous or separate cells can be solved.