325.10R-95: Report on Roller-Compacted Concrete Pavements (Reapproved 2001)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 325.10R-95: Report on Roller-Compacted Concrete Pavements (Reapproved 2001)

Author(s): ACI Committee 325

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 32

Keywords: pavements

DOI:

Date: 3/1/1995

Abstract:
This report covers the present state of the art for roller-compacted concrete pavements. It contains information on applications, material properties, mix proportioning, design, construction, and quality control procedures. Roller-compacted concrete use for pavements is relatively recent and the technology is still evolving. The pavement consists of a relatively stiff mixture of aggregate, cementitious materials and water, that is compacted by rollers and hardened into concrete.