311.5R-97: Guide for Concrete Plant Inspection and Field Testing of Ready-Mixed Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 311.5R-97: Guide for Concrete Plant Inspection and Field Testing of Ready-Mixed Concrete

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 5

Keywords: inspection

DOI:

Date: 10/16/1997

Abstract:

Note: A newer version of this document exists. This document was replaced by 311.5-02.

This guide is intended for use in establishing only the most basic duties and reports required of inspection personnel. It can be used for all types and sizes of projects, but should be supplemented with additional inspection requirements when the complexity of the project so dictates. Refer to "Guide for Concrete Inspection Programs" (ACI 311.4R) for guidance on additional requirements. This guide recommends minimum requirements for inspection at the concrete plant when such inspections are required by specifications or the owner. It is intended for use by specifiers, architects, engineers, owners, contractors or other groups needing to monitor the ready-mixed concrete producers' activities at the concrete plant through the use of an independent inspection agency or in-house inspection organization. This guide also recommends minimum inspector qualifications, duties and reports.