309.2R-98: Identification and Control of Visible Effects of Consolidation on Formed Concrete Surface

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 309.2R-98: Identification and Control of Visible Effects of Consolidation on Formed Concrete Surface

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 11

Keywords: consolidation

DOI:

Date: 8/19/1998

Abstract:

Note: A newer version of this document exists. This document was replaced by 309.2R-15.

This report provides guidelines for identifying and controlling visible effects of consolidation on precast or cast-in-place formed concrete surfaces. It includes a summary of direct and indirect causes of such imperfections. An outline to assist in the reporting on surfaces and photographs to illustrate typical concrete blemsihes are also included.