Title: 303R-91: Guide to Cast-in-Place Architectural Concrete Practice

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 30

Keywords: architectural concrete

DOI:

Date: 11/1/1991

Abstract:

Note: A newer version of this document exists. This document was replaced by 303R-04.

Recommendations for the production of cast-in-place architectural concrete. The importance of specified materials, forming, concrete placement, curing, additional treatment, inspection and their effect on finished product is discussed.