224R-90: Control of Cracking in Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 224R-90: Control of Cracking in Concrete Structures

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 43

Keywords: cracking

DOI:

Date: 1/1/1990

Abstract:

Note: A newer version of this document exists. This document was replaced by 224R-01.

The principal causes of cracking in concrete and recommended crack control procedures are presented. The current state of knowledge in microcracking and fracture mechanics is discussed. The control of cracking due to drying shrinkage and crack control for flexural members, layered systems and mass concrete are covered in detail. Long-term effects on cracking are considered, and crack control procedures used in construction are presented. Information is provided to assist the engineer and the constructor in developing practical and effective crack control programs for concrete structures.