212.4R-93: Guide for the Use of High-Range Water-Reducing Admixtures (Superplasticizers) in Concrete (Reapproved 1998)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 212.4R-93: Guide for the Use of High-Range Water-Reducing Admixtures (Superplasticizers) in Concrete (Reapproved 1998)

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 10

Keywords: admixtures

DOI:

Date: 7/1/1993

Abstract:

Note: A newer version of this document exists. This document was replaced by 212.4R-04.

The use of high-range water-reducing admixtures is increasing substantially in the concrete industry. They are used to increase strength of concrete and provide greatly increased workability without the addition of excessive amounts of water. This guide contains information on application, uses, and effects on freshly mixed and hardened water-reducing admixtures. The guide is designed for use by concrete suppliers, contractors, designers, specifiers, and all others engaged in concrete construction.