211.1-91: Standard Practice for Selecting Proportions for Normal, Heavyweight and Mass Concrete (Reapproved 2009)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 211.1-91: Standard Practice for Selecting Proportions for Normal, Heavyweight and Mass Concrete (Reapproved 2009)

Author(s): ACI Committee 211

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 38

Keywords: proportioning

DOI:

Date: 11/1/1991

Abstract:
This publication describes methods for selecting and adjusting proportions for normal weight concrete. The procedures take into consideration the requirements for placability, consistency, strength, and durability. Example calculations are shown including adjustments based on the characteristics of the first trial batch. The proportioning of heavyweight concrete for such purposes as radiation shielding and bridge counterweight structures is described.