Comparative Statistical Study for the Ultimate Stress in Unbonded PostTensioning

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Comparative Statistical Study for the Ultimate Stress in Unbonded PostTensioning

Author(s): Jeffrey M. Ament, P. R. Chakrabarti, and C. S. Putcha

Publication: Structural Journal

Volume: 94

Issue: 2

Appears on pages(s): 171-180

Keywords: post-tensioning; regression analysis; standard deviation; stresses; unbonded prestressing;

DOI: 10.14359/471

Date: 3/1/1997

Abstract:
In this paper an attempt is made to make a statistical study of the accuracy of various equations for prediction of the ultimate stress of unbonded prestressed beams (fps) suggested by different investigators in recent years. Comparison is made with the experimental results. Comparison is also made with ACI 31889/92 code equations (184) and (185). Each equation is tested using the combined pool of all the experimental data used by these investigators.