Super High-Story Pumping: Shanghai Jin Mao Building

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Super High-Story Pumping: Shanghai Jin Mao Building

Author(s): Cao Tian Xia

Publication: Concrete International

Volume: 22

Issue: 5

Appears on pages(s): 55-59

Keywords:

DOI:

Date: 5/1/2000

Abstract:
Continuous placement of 80,200 m3 (105,000 yd3) of concrete to a height of 450 m (1476 ft) in construction of third highest building in the world. Specially selected concrete mixture used in mass concrete foundation placement. Author describes continuous placement of HSC in mass concrete mat foundation. Optimized mixture and temperature controls addressed.