Strengthening of Initially Loaded Reinforced Concrete Beams Using FRP Plates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strengthening of Initially Loaded Reinforced Concrete Beams Using FRP Plates

Author(s): Alfarabi Sharif, G. J. Al-Sulaimani, I. A. Basunbul, M. H. Baluch, and B. N. Ghaleb

Publication: Structural Journal

Volume: 91

Issue: 2

Appears on pages(s): 160-168

Keywords: adhesives; beams (supports); ductility; flexural strength; composite construction (concrete and plastic); composite construction (concrete and steel); Structural Research

DOI: 10.14359/4594

Date: 3/1/1994

Abstract:
The repair of initially jacketed reinforced concrete (RC) beams with epoxy-bonded fiberglass reinforced plastic (FRP) plates is experimentally investigated. The RC beams are initially loaded to 85 percent of the ultimate flexural capacity and subsequently repaired with FRP plates bonded to the soffit of the beam. The jacket thickness is varied to assess the premature failure initiated at the plate curtailment zone due to the high concentration of shear and peeling stresses. Different repair and anchoring schemes are conducted in an effort to eliminate such failures and insure ductile behavior. The behavior of the repaired beams is represented by load-deflection curves and the different modes of failure are discussed. The results generally indicate that the flexural strength of the repaired beams is increased. The ductile behavior of the repaired beams is inversely proportional to the plate thickness. The use of an I-jacket plate provided a proper anchorage system and improved the ductility of beams repaired with plates of large thickness.