Application of Ferrocement in Bridge Engineering--China

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Application of Ferrocement in Bridge Engineering--China

Author(s): Ding Dajun

Publication: Concrete International

Volume: 16

Issue: 4

Appears on pages(s): 40-43

Keywords: bridge foundations; bridges (structures); caissons; ferrocement; girders; pavements; piles; Materials Research

DOI:

Date: 4/1/1994

Abstract:
In China, ferrocement has been used for many years in bridge construction. Examples of such applications include two-way curved shallow shells, two-way curved shells for formwork, where stones are incorporated in the construction of two-way composite arches, thin-walled slabs for box beams, stiffeners for box girders in long-span suspension bridges, floating thin-walled caissons for bridge piers, and protective tubes for piles.