Reactive Powder Concretes With High Ductility and 200 - 800 Mpa Compressive Strength

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reactive Powder Concretes With High Ductility and 200 - 800 Mpa Compressive Strength

Author(s): P. Richard and M. H. Cheyrezy

Publication: Symposium Paper

Volume: 144

Issue:

Appears on pages(s): 507-518

Keywords: cement pastes; compressive strength; concretes; density (mass/volume); ductility; flexural strength; high-strength concretes; microstructure; silica fume; strength; structural members; General

DOI: 10.14359/4536

Date: 3/1/1994

Abstract:
The use of ultra-high-strength concrete for the construction of some types of structural members can be considered if nonbrittle behavior is achieved. Paper introduces reactive powder concretes (RPC) that exhibit ultra-high strength and high ductility at the same time. Compared to conventional concretes, the ductility estimated in terms of fracture energy is increased by one to two orders of magnitude, while the compressive strength values are in the range of 200 to 800 MPa..




  