Use of Laboratory Techniques to Evaluate Long-Term Durability of Steel-Reinforced Concrete Exposed to Chloride Ingress

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use of Laboratory Techniques to Evaluate Long-Term Durability of Steel-Reinforced Concrete Exposed to Chloride Ingress

Author(s): N. S. Berke

Publication: Symposium Paper

Volume: 145

Issue:

Appears on pages(s): 299-330

Keywords: chlorides; concretes; corrosion; corrosion tests; diffusion; durability; reinforced concrete; reinforcing steels; spectroscopy; tests; Structural Research

DOI: 10.14359/4467

Date: 5/1/1994

Abstract:
The corrosion of steel in reinforced concrete due to the ingress of chlorides is a major cause for the decreased durability of structures built in marine and deicing salt environments. A multitude of research has been conducted to evaluate the corrosion of steel in concrete and to develop protection systems to arrest this process. This paper critically discusses some of the more popular techniques and presents new data illustrating the importance of selecting the right corrosion tests.