Influence of Dimension of Test Specimen on Alkali- Aggregate Reactive Expansion

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Dimension of Test Specimen on Alkali- Aggregate Reactive Expansion

Author(s): Chengzhi Zhang, Aiqin Wang, Mingshu Tang, and Ningsheng Zhang

Publication: Materials Journal

Volume: 96

Issue: 2

Appears on pages(s): 204-207

Keywords: alkali-aggregate reactions; heat transfer; mortars

DOI: 10.14359/446

Date: 3/1/1999

Abstract:
The influence of the dimension of test specimen on the expansion of both alkali-silica reaction (ASR) and alkali-carbonate reaction (ACR) is studied in the paper. The results show that the dimension of test specimen influences markedly ASR expansion, but not ACR expansion. For ASR expansion, the larger the aggregate, the greater the influence of the test specimen dimension is. From two processes of the transference of heat and the transference of mass, why the dimension of test specimen influences alkali-aggregate reactive (AAR) expansion is analyzed. The loss of the activated compound in the aggregate is an important reason.