Effect of Deformation Height and Spacing on Bond Strength of Reinforcing Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Deformation Height and Spacing on Bond Strength of Reinforcing Bars

Author(s): David Darwin and Ebenezer K. Graham

Publication: Structural Journal

Volume: 90

Issue: 6

Appears on pages(s): 646-657

Keywords: bond (concrete to reinforcement); deformed reinforcement; pullout tests; reinforcing steels; structural engineering; Structural Research

DOI: 10.14359/4459

Date: 11/1/1993

Abstract:
The effect of deformation pattern on bond strength is studied using 1-in. (25-mm) diameter machined bars with deformation heights of 0.05, 0.075, and 0.10 in. (1.27, 1.91, and 2.54 mm) and deformation spacings ranging from 0.26 to 2.2 in. (6.7 to 56 mm). The combination of rib height and spacing produce relative rib areas (ratio of projected rib area normal to bar axis to product of nominal bar perimeter and center-to-center rib spacing) of 0.20, 0.10, and 0.95 for each deformation height. Conventional reinforcing bars, with a relative rib area of 0.07, are also studied. The effect of deformation pattern is evaluated using beam-end specimens with varying degrees of confinement provided to the test bars. Degrees of confinement are: 1) 2-in. (51-mm) cover without transverse stirrups, 2) 2-in. (51-mm) cover with confining transverse stirrups, and 3) 3-in. (76-mm) cover without confining transverse stirrups. Bars with 2-in. (51-mm) cover have an initial unbonded length of -1/2 in. (13 mm) and a bonded length of 12 in. (305 mm). Bars with 3-in. (76-mm) cover have an initial unbonded length of 4 in. (102 mm) and a bonded length of 8-1/2 in. (216 mm). The bond force-slip response of reinforcing bars is a function of the relative rib area of the bars, independent of the specific combination of rib height and rib spacing. Under all conditions of bar confinement, the initial stiffness of load-slip curves increases with an increase in the relative rib area. Under conditions of relatively low confinement, in which bond strength is governed by splitting of the concrete, bond strength is independent of deformation pattern. Under conditions in which additional bar confinement is provided by transverse reinforcement or higher cover, bond strength increases compared to the bond strength of bars with less confinement. The magnitude of the increase in bond strength increases with an increase in the relative rib area.


ALSO AVAILABLE IN:

Electronic Structural Journal