Durability Studies of Concrete Containing Low Cement Content and Fine Particles of Foundry Slag

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Durability Studies of Concrete Containing Low Cement Content and Fine Particles of Foundry Slag

Author(s): S. I. Pavlenko and V. S. Bogusevich

Publication: Symposium Paper

Volume: 145

Issue:

Appears on pages(s): 1069-1086

Keywords: acids; admixtures; air-entrained concretes; cement content; concretes; corrosion; creep properties; deformation; diffusion; tests; drying shrinkage; durability; freeze-thaw durability; permeability; sands; slags; Materials Research

DOI: 10.14359/4425

Date: 5/1/1994

Abstract:
The Siberian Metallurgical Institute (SMI) has developed low-cement concrete with acid and basic slags from a Russian foundry. The concrete contains neither natural aggregates (crushed stone, gravel, or sand) nor artificial porous aggregates (claydite, aggloporite, polystyrene, or others). It includes the following materials: 680 to 1140 kg/m 3 of acid slag sand form PTP with a particle size of 0 to 5 mm used as fine aggregate; cementitious materials (340 to 400 kg/m 3 of fine-grained basic slag and 100 to 170 kg/m 3 of M500 portland cement); 260 to 290 kg/m 3 of water; 0.3 percent by weight of cement of plasticizing admixture (technical grade lignosulfonate); and 1 to 2 percent of air-entraining admixture (secondary sodium alkyl sulfate). To make the wide application of this concrete possible in construction (mainly for low-rise cottages), deformation properties, protection of reinforcement from corrosion, frost resistance, and water and gas permeability were studied during a 1-year period. The investigation shows that concrete developed in this way complies with Russian international standards for low-strength concrete and can be used in housing construction. Air-entrained concrete for external walls should be protected by mortar or some other finishing material.