Durability Factors Affecting CLSM

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Durability Factors Affecting CLSM

Author(s): W. E. Brewer

Publication: Symposium Paper

Volume: 150

Issue:

Appears on pages(s): 39-52

Keywords: backfilling; controlled low-strength material (CLSM); corrosion; compression; durability; flowability; fly ash; pavements; permeability; quality assurance; quality control; strength; General

DOI: 10.14359/4386

Date: 6/1/1994

Abstract:
Paper covers various aspects of controlled low-strength material (CLSM) and discusses CLSM's durability factors. It reviews CLSM's early history, listing possible uses and applications. Quality assurance and quality control compaisons are made between conventional portland cement concrete and CLSM. CLSM durability factors are referenced for each possible use and application, and tests are listed for CLSM's durability and methods to insure this durability.