Reduced Strand Spacing in Pretensioned, Prestressed Members

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reduced Strand Spacing in Pretensioned, Prestressed Members

Author(s): Thomas E. Cousins, J. Michael Stallings, and Michael B. Simmons

Publication: Structural Journal

Volume: 91

Issue: 3

Appears on pages(s): 277-286

Keywords: bonding; building codes; prestressed concrete; prestressing steels; pretensioning; stress transfer; Structural Research

DOI: 10.14359/4359

Date: 5/1/1994

Abstract:
Pretensioned, prestressed concrete girders are used widely in bridge superstructures in the United States. Predominantly, 0.5-in. (12.7-mm)-diameter prestressing strand is used in these girders at a center-to-center spacing of 2 in. (50.8 mm). This corresponds to the four-strand-diameter center-to-center spacing, which is the ACI 318-89 minimum requirements for pretensioned, prestressed members. In the past, however, several states have used a center-to-center strand spacing of 1.75 in. (44.5 mm) with success. The purpose of this paper is to report the results of laboratory tests designed to determine if the closer strand spacing has a detrimental effect on prestressed girder performance. Twelve test specimens were cast for the study, six with the 1.75-in. (44.5-mm) strand spacing and six with the 2-in. (50.8-mm) strand spacing. The experimental results from this research were compared to results in the literature and the provisions of the ACI Building Code (ACI 318-89). It was concluded that the closer strand spacing has no significant effect on transfer length, development length, or nominal moment capacity.