Title: Call for Standardized Tests for Corrosion-Inhibiting Admixtures Corrosion-Inhibiting Admixtures; Corrosion; Corrosion Resistance; corrosion tests; reinforced Concrete; General

Author(s): Paul Tourney and Neal Berke

Publication: Concrete International

Volume: 15

Issue: 4

Appears on pages(s): 57-62

Keywords: corrosion-inhibiting admixtures; corrosion; corrosion resistance; corrosion tests; reinforced concrete; General

DOI:

Date: 4/1/1993

Abstract:
Discusses the need for standardized tests for corrosion-inhibiting admixtures. Describes suitable test procedures and discusses their importance.