Title: High-Strength Concrete in China

Author(s): Jiang Jiafen

Publication: Concrete International

Volume: 15

Issue: 1

Appears on pages(s): 43-45

Keywords: brittleness; high-strength concretes; mechanical properties; physical properties; silica fume; superplasticizers; General

DOI:

Date: 1/1/1993

Abstract:
Brief introduction to some achievements in the field of high-strength concrete in China is presented, particularly during the past 10 years. The development, application, preparation, and physical and mechanical properties are described concisely.