Mechanism of Rupture in Splitting Test

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mechanism of Rupture in Splitting Test

Author(s): Claudio Rocco, Gustavo V. Guinea, Jaime Planas, and Manuel Elices

Publication: Materials Journal

Volume: 96

Issue: 1

Appears on pages(s): 52-60

Keywords: concretes; crack propagation; granite; mortars; tensile strength

DOI: 10.14359/428

Date: 1/1/1999

Abstract:
The fracture mechanisms in the splitting tensile test (Brazilian test) are studied experimentally with special attention given to the influence of the width bearing strips. Tests of an extended size range (1:10) were conducted on mortar square prisms and on granite discs. The tests were carried out on a closed-loop control system to obtain stable crack propagation. During the tests, crack initiation and propagation were recorded. The results confirm the existence of two fracture mechanisms in the splitting test: one associated with development of central cracks, and the other with a secondary crack system on both sides of the bearing strips. These secondary cracks appear as a consequence of the stress redistribution induced by the central crack growth. The load-displacement curves recorded during the stable test show that two peak loads exist, one for each mechanism. The relative values of these peak loads depend on the specimen size and on the width of the bearing strip; with a smaller size and a wider bearing strip, the relative value of the peak load associated with the secondary crack system increases.