Workability Characteristics of High-Strength Concrete Incorporating an Air-Entraining, High-Range Water-Reducing Admixture

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Workability Characteristics of High-Strength Concrete Incorporating an Air-Entraining, High-Range Water-Reducing Admixture

Author(s): M. Kayaga, H. Tokuda, M. Kawakami, and T. Kaneko

Publication: Symposium Paper

Volume: 148

Issue:

Appears on pages(s): 121-130

Keywords: admixtures; air-entraining agents; compaction; workability; compressive strength; consolidation; high-strength concretes; segregation; slump; vibrators (machinery); water-reducing agents; General

DOI: 10.14359/4275

Date: 9/1/1994

Abstract:
High-strength concrete with air-entraining high-range water-reducing admixture, 0.35 water-cement ratio, 148 kg/m 3 unit water content, and about 60 MPa compressive strength, was produced, and the admixture content and sand percentage were varied. The consistency property was measured by the slump test, and the compaction property and segregation resistance were determined by the flow time through an inverted slump cone. An appropriate mixture that balanced these properties relative to the admixture content and sand percentage was determined from the test. The appropriate mixture can be consolidated by using a shorter vibrating time and lower frequency than in the case of ordinary concrete.