Building the United States' Largest Concrete Caisson

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Building the United States' Largest Concrete Caisson

Author(s): Todd Watson

Publication: Concrete International

Volume: 15

Issue: 3

Appears on pages(s): 55-57

Keywords: caissons; clay soils; formwork (construction); piles; shoring; pumped concrete; tunnels; vibration; waste treatment; Construction

DOI:

Date: 3/1/1993

Abstract:
Construction on what may be the largest concrete caisson in the United States will soon be completed in Detroit, Michigan. The self-sinking, 140 ft diameter, 82 ft tall circular caisson will house seven pumps, each capable of moving 107 million gal per day of raw sewage. Walbridge Aldinger is the general contractor constructing the caisson as part of an expansion of the Detroit Water and Sewerage Department's (DWSD) Wastewater Treatment Plant.