Title: Installing and Testing Large Adhesive anchors

Author(s): John Beebe and Robert R. McGlohn

Publication: Concrete International

Volume: 15

Issue: 5

Appears on pages(s): 61-65

Keywords: adhesives; anchor bolts; epoxy resins; foundations; tests; Construction

DOI:

Date: 5/1/1993

Abstract:
Describes project to reinforce and reuse an existing foundation for two boiler stacks that were being heightened by 62 ft. Article focuses on the installation and testing program for anchor bolts required to reinforce the foundation.