Post-Tensioned Industrial floors

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Post-Tensioned Industrial floors

Author(s): Miroslav Vejvoda

Publication: Concrete International

Volume: 15

Issue: 1

Appears on pages(s): 53-55

Keywords: concrete slabs; construction joints; control joints; cracking; flat concrete slabs; post-tensioning; slab-on-ground construction; Design

DOI:

Date: 1/1/1993

Abstract:
Discusses the use of post-tensioning in industrial concrete slabs-on-grade for controlling cracks, reducing the number of joints, reducing the slab thickness, and lowering maintenance costs. Provides four examples of post- tensioned slabs with various flatness requirements and joint configurations.