Creep compensating prestress of tanks

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Creep compensating prestress of tanks

Author(s): Troels Brondum-Nielsen

Publication: Structural Journal

Volume: 90

Issue: 1

Appears on pages(s): 32-36

Keywords: bending moments; circular prestressing; creep properties; prestressed concrete; stress analysis; stress relaxation; structural design; tanks (containers); Structural Research

DOI: 10.14359/4192

Date: 1/1/1993

Abstract:
The adverse effects of stress redistribution due to creep (or concrete stress relaxation) can be reduced by prestressing. Suggests a different, and apparently more economical, distribution of the circumferential prestress than that conventionally adopted.


ALSO AVAILABLE IN:

Electronic Structural Journal