Title: High-Performance Concrete Columns

Author(s): N. A. Lloyd and B. V. Rangan

Publication: Symposium Paper

Volume: 149

Issue:

Appears on pages(s): 379-390

Keywords: columns (supports); compressive strength; failure; high-performance concretes; loads (forces); reinforced concrete; strength; Structural Research

DOI: 10.14359/4167

Date: 10/1/1994

Abstract:
Presents the results obtained from tests on high-performance concrete columns. Twenty-four columns were tested. The test parameters included shape and size of cross section, longitudinal reinforcement ratio, load eccentricity, and concrete compressive strength. Analytical methods to predict the behavior and strength of columns are also presented. Good correlation between test and analytical results is found.