Study of Reinforcing Detail of Tension Bars in Frame Corner Connections

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Study of Reinforcing Detail of Tension Bars in Frame Corner Connections

Author(s): Y. H. Luo, A. J. Durrani, Shaoliang Bai, and Jixing Yuan

Publication: Structural Journal

Volume: 91

Issue: 4

Appears on pages(s): 486-496

Keywords: frames; lap connections; reinforced concrete; Structural Research

DOI: 10.14359/4156

Date: 7/1/1994

Abstract:
Twenty-seven full-scale frame corners were tested under monotonic closing load to study the effect of reinforcing detail on the performance of beam-to-column knee connection. The failure mechanism, crack patterns of the frame corners, strain distribution in the tension bars along the lap length, and the load-carrying capacity of the specimens are presented. Based on the observed behavior of corner connections, it is concluded that improper detailing could significantly affect the strength and ductility of the beam-to-column knee connections.


ALSO AVAILABLE IN:

Electronic Structural Journal