Flexural behavior including ductility of high-strength Lightweight Concrete Members Under Reversed Cyclic Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexural behavior including ductility of high-strength Lightweight Concrete Members Under Reversed Cyclic Loading

Author(s): S. K. Ghosh, D. P. Narielwala, S. W. Shin, and J. Moreno

Publication: Symposium Paper

Volume: 136

Issue:

Appears on pages(s): 357-376

Keywords: cyclic loads; deflection; ductility; flexural strength; high-strength concretes; hysteresis; lightweight concrete; reinforced concretes; shear properties; yield strength; Structural Research

DOI: 10.14359/4129

Date: 1/1/1993

Abstract:
This experimental investigation was aimed at gathering information on flexural properties, including ductility, of high-strength lightweight concrete members (concrete with a dry unit weight of approximately 120 lb/ft 3 and with compressive strength approaching 9 ksi at 56 days) under reversed cyclic loading. Two sets of six specimens each were manufactured using lightweight aggregate concrete having compressive strengths of 5 ksi at 28 days and 9 ksi at 56 days. The test variables were concrete strength, amount of longitudinal reinforcement, and spacing of ties. The test results, including hysteretic load-deflection curves, for specimens representing columns under zero axial load are reported.