Computer Analysis of Reinforced Concrete Sections Under Biaxial Bending and Longitudinal Load

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Computer Analysis of Reinforced Concrete Sections Under Biaxial Bending and Longitudinal Load

Author(s): M. L. Zak

Publication: Structural Journal

Volume: 90

Issue: 2

Appears on pages(s): 163-169

Keywords: bending; biaxial loads; computer programs; concretes; equilibrium; loads (forces); reinforced concrete; reinforcing steels; strains; strength; stress-strain relationships; structural analysis; Structural Research

DOI: 10.14359/4122

Date: 3/1/1993

Abstract:
insures convergence of the iterations to the equilibrium equations solution by any mode of loading. For computation of the coefficients in the equilibrium equations, a version of the fictitious-domain method is proposed, which allows essentially treatment of rectangular and nonrectangular sections in the same way, and makes the presented approach easily programmable and readily adaptable to different sections. An additional procedure is suggested for analysis of more difficult cases, when the strain in the extreme compression fiber of the section is considered as a variable that is not specified in advance. Numerical examples are given.