Effect of Reinforcement Ratio on the Effective Moment of Inertia of Reinforced Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Reinforcement Ratio on the Effective Moment of Inertia of Reinforced Concrete Beams

Author(s): Abdulrahman H. Alshaikh and Rajeh Al-Zaid

Publication: Structural Journal

Volume: 90

Issue: 2

Appears on pages(s): 144-149

Keywords: beams (supports); deflection; moment of inertia; reinforced concrete; reinforcement ratio; Structural Research

DOI: 10.14359/4119

Date: 3/1/1993

Abstract:
Test results with values obtained using the ACI Building Code equation of the effective moment of inertia showed a noticeable difference, especially for heavily reinforced sections. The difference was accounted for by modifying the exponent in the effective moment of inertia equation. The effect of using the moment of inertia of the uncracked transformed section in the computation of the effective moment of inertia was also discussed. In addition, the effect of the reinforcement ratio was incorporated in a recently developed model which estimates the effective moment of inertia of reinforced concrete beams under any type of symmetrical loading by considering the variation in the beam's cracked length.