High-Performance Concrete: Low-Heat and High-Strength

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: High-Performance Concrete: Low-Heat and High-Strength

Author(s): K. Sakai and H. Watanabe

Publication: Symposium Paper

Volume: 149

Issue:

Appears on pages(s): 243-268

Keywords: admixtures; blast furnace slag; carbonation; compressive strength; high-performance concretes; low-heat cements; porosity; temperature; Materials Research

DOI: 10.14359/4082

Date: 10/1/1994

Abstract:
Basic studies were conducted to develop high-performance concrete, with low-heat and high-strength characteristics under low-temperature environments, using blast furnace slag. The purpose of this study was to clarify the effects of slag fineness, slag content, gypsum content, limestone-powder content, and high-range water-reducing admixtures (HRWRA) on the strength development, adiabatic temperature rise, porosity, amount of Ca(OH) 2, and carbonation of concrete; and the effect of curing temperature on concrete strength development. As a result of this study, it was found that it is possible to produce high-performance concrete with low heat and high strength under low-temperature environments, by properly combining, and taking into consideration, their respective properties, granulated blast furnace slag, HRWRA, and other admixtures.