Low-Strength Concrete and Controlled Low-Strength Material (CLSM) Produced With Class F Fly Ash

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Low-Strength Concrete and Controlled Low-Strength Material (CLSM) Produced With Class F Fly Ash

Author(s): T. R. Naik and B. W. Ramme

Publication: Symposium Paper

Volume: 150

Issue:

Appears on pages(s): 1-14

Keywords: backfilling; compressive strength; controlled low-strength material (CLSM); density (mass/volume); flowability; flowable fill; fly ash; low-strength concrete; mix proportioning; slump; slurries; tests; Materials Research

DOI: 10.14359/4071

Date: 6/1/1994

Abstract:
Presents results of research performed to identify optimum mix proportions for production of controlled low-strength materials (CLSM) with high fly ash content. CLSM is defined by ACI Committee 229 as a cementitious material that is in a flowable state at the time of placement, with a specified compressive strength of 1200 psi (8.3 MPa or 172,800 psf) or less at 28 days. The fly ash used in this study met the requirements of ASTM C 618 for Class F material. Tests were carried out on concrete designed for 500 to 1500 psi compressive strength at 28 days, with fly ash contents of approximately 500 lb/yd 3. Slump was held at 8 ¦1 in. for all mixes produced. Compressive strengths at 28 days were found to range from 290 to 1640 psi. Construction experience and other planned applications are also discussed. 141-494