Title: Guide to Portland Cement Plastering

Author(s): ACI Committee 524

Publication: Materials Journal

Volume: 90

Issue: 1

Appears on pages(s): 69-93

Keywords: accessories; admixtures; application; bases; bond; brown coat; cement; color; cracking (fracturing); curing; finish coat; furring; masonry; metal lath; mixing; plaster; proportioning; reinforcement; scratch coat; shrinkage; stucco; texture; Materials Res

DOI: 10.14359/4043

Date: 1/1/1993

Abstract:
Guide is an update of ACI 524, "Guide to Portland Cement Plastering," which was published in 1964. There are a number of revisions reflecting increased knowledge of plaster and the use of current materials and methods. Recommendations for producing good portland cement-based plaster are described. Various characteristics, procedures, and alternates with advantages and disadvantages are given.