Title: Analytical Formulation of the Biaxial Behavior of Concrete Repair Material

Author(s): George Z. Voyiadjis and Taher M. Abulebdeh

Publication: Materials Journal

Volume: 90

Issue: 1

Appears on pages(s): 26-33

Keywords: biaxial loads; brittleness; concretes; loads (forces); repairs; patching; strength; Structural Research

DOI: 10.14359/4023

Date: 1/1/1993

Abstract:
An analytical investigation into the behavior of concrete under tension-compression stress states is described. Analytical expressions are developed to predict the ultimate strength envelope as well as the peak stress and the corresponding strain. Analytical stress-strain relations for repaired system under biaxial loading are derived. The proposed analytical expression provides good agreement between the available experimental and analytical stress-strain curves.