Experimental and Numerical Analysis of High Strain Rate Splitting-Tensile Tests

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental and Numerical Analysis of High Strain Rate Splitting-Tensile Tests

Author(s): Joseph W. Tedesco and C. Allen Ross

Publication: Materials Journal

Volume: 90

Issue: 2

Appears on pages(s): 162-169

Keywords: concretes; cracking (fracturing); dynamic loads; tensile strength; splitting tensile strength; strains; Materials Research

DOI: 10.14359/4013

Date: 3/1/1993

Abstract:
Splitting-tensile concrete specimens were tested at strain rates of 10 -7/sec to 10 2 in a low-speed material test and in a 50.8-mm (2-in.) diameter split-Hopkinson pressure bar (SHPB). A comprehensive finite element method (FEM) analysis was conducted on these same test specimens. A high-speed framing camera (10,000 frames/sec) was used to record the gross deformation and cracking during the fracture process in the SHPB tests. In addition, an ultra- high-speed image converter camera with equivalent framing rates of 10,000 to 1,000,000 frames/sec was used to record some of the early crack formations during the fracture process in the SHPB tests. Results of tensile strength versus strain-rate are presented and compared with compressive strength at similar strain-rates. These same tensile data are compared with strength data obtained using a fracture mechanics model. Computer-generated crack patterns are presented and compared to experimentally observed crack patterns in the fracture of concrete at high strain-rates.


ALSO AVAILABLE IN:

Electronic Materials Journal