Ponckhockie Union Chapel--1870

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ponckhockie Union Chapel--1870

Author(s): Raymond C. Heun

Publication: Concrete International

Volume: 15

Issue: 10

Appears on pages(s): 69-70

Keywords: aggregates; cement lime mortars; concrete construction; durability; lime cements; portland cements; reinforced concrete; General

DOI:

Date: 10/1/1993

Abstract:
Constructed in 1870, the Ponckhockie Union Chapel in the Roundout section of Kingston, New York, is the oldest reinforced concrete structure in the United States. It is the culmination of early efforts on the part of a new industry--the concrete industry.