How Soon is Soon Enough? Revisited

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: How Soon is Soon Enough? Revisited

Author(s): Bryant Mather

Publication: Symposium Paper

Volume: 141

Issue:

Appears on pages(s): 1-10

Keywords: age-strength relation; building codes; concrete construction; concretes; fresh concretes; mix proportioning; quality control; specifications; tests; General

DOI: 10.14359/3987

Date: 12/1/1993

Abstract:
The customary criterion for establishing grades of structural concrete is the crushing strength measured in an arbitrary manner on a standardized specimen stored in a stipulated fashion for approximately a month after making. In some parts of the world, the specimen is a cube, and in other parts of the world, the specimen is a cylinder. There have been debates as to how the strength at 28 days can be predicted from procedures performed at early ages, especially 24 hr, on the grounds that a month is not soon enough. The intent of this paper is to suggest that the only time that really is "soon enough" to know that the grade of the concrete in any batch is correct is before the concrete is discharged from the concrete mixer into the forms. It is suggested, therefore, that effort would preferably be expended upon insuring that the materials used are those intended and the proportions in which they are used are those that were intended. If this is the case, the grade of concrete will be proper at all ages, and testing at any age is merely confirmation.