Title: Direct Determination of Tension Development Lengths of Beam Flexural Reinforcement

Author(s): Douglas Dongwoo Lee

Publication: Concrete International

Volume: 15

Issue: 8

Appears on pages(s): 50-54

Keywords: beams (supports); cover; flexural strength; reinforcing steels; stirrups; structural design; Design

DOI:

Date: 8/1/1993

Abstract:
With an increased number of multipliers for tension development of reinforcement in ACI 318-89, designers have found the determination of tension development lengths very tedious and time-consuming. A design aid is developed for typical beams to determine tension development lengths directly from tables without any calculations.