Estimating the Service Life of Epoxy Coated Reinforcing Steel

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Estimating the Service Life of Epoxy Coated Reinforcing Steel

Author(s): Richard E. Weyers Wioleta Pul, and Michael M. Sprinkel

Publication: Materials Journal

Volume: 95

Issue: 5

Appears on pages(s): 546-557

Keywords: coating debondment; corrosion mechanism; corrosion protection; cost-effectiveness; epoxy resins;

DOI: 10.14359/397

Date: 9/1/1998

Abstract:
Corrosion protection performance of fusion bonded epoxy coated reinforcing steel (FBECR) was evaluated in chloride doped simulated concrete pore water solutions and field structures. Results demonstrate that different corrosion protection failure mode exists in the field than in short-term laboratory studies.In laboratory studies, the chloride is at the bar surface area immediately and the degree of corrosion protection is a function of the quality of the coating. In field structures, the epoxy coating debonds from the steel in moist-wet concrete. The rate of epoxy debondment and the chloride increase at the bar depth determine if the chloride corrosion threshold limit is reached before or after the epoxy debonds. If the coating is debonded when the chlorides reach the corrosion threshold limit corrosion takes place under the coating in an acidic environment and the corrosion protection of FBECR is nil. In Virginia, FBECR may provide protection for about 5 percent of the bridge decks and thus FBECR may not be a cost effective corrosion protection system for Virginia bridges.


ALSO AVAILABLE IN:

Electronic Materials Journal