Flexural Performance of Concrete Beams Reinforced With Continuous Fiber Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexural Performance of Concrete Beams Reinforced With Continuous Fiber Bars

Author(s): K. Nakano, Y. Matsuzaki, H. Fukuyama, and M. Teshigawara

Publication: Symposium Paper

Volume: 138

Issue:

Appears on pages(s): 743-766

Keywords: beams (supports); compressive strength; ductility; fibers; flexural strength; prestressed concrete; prestressing steels; reinforced concrete; reinforcing steels; tensile properties; tensile strength; Structural Research

DOI: 10.14359/3955

Date: 9/1/1993

Abstract:
An experimental investigation was carried out to study and evaluate the flexural performance of concrete beams reinforced with continuous fiber bars (main reinforcing bars and prestressing tendons). Two series of flexural tests were conducted, and the primary variables were fiber material, tensile reinforcement ratio, concrete compressive strength, and bond condition in prestressing tendon. Through this experimental study, the following facts were clarified. The flexural performance of concrete beams reinforced with continuous fiber bars can be evaluated by conventional methods used in concrete beams reinforced with steel bars. The ductility capacity of reinforced concrete beams can be controlled by the compressive failure of concrete, and in prestressed concrete beams, can be controlled by changing unbonded length of prestressing tendon.