Finite Element Analysis of High-Strength Concrete Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Finite Element Analysis of High-Strength Concrete Slabs

Author(s): H. M. Marzouk and Zhiwei Chen

Publication: Structural Journal

Volume: 90

Issue: 5

Appears on pages(s): 505-513

Keywords: high-strength concrete; finite element method; fly ash; offshore structures; plasticity; punching shear; shells (structural forms); silica fume; slabs; tension; Structural Research

DOI: 10.14359/3943

Date: 9/1/1993

Abstract:
Presents an analytical investigation on the behavior of reinforced high-strength concrete slabs. A plasticity-based concrete model is used for the finite element analysis. An eight-node quadrilateral shell element with a reduced 2 x 2 Gaussian integration over the element plane and nine-point Simpson-type integration through the element thickness are employed. A suitable post-cracking tensile model of reinforced high-strength concrete is utilized, based on the fracture energy of high-strength concrete recorded from stress-displacement curves (stress-crack width curves). The validity of the developed model is then established by comparison with the results of reinforced high-strength concrete slabs. Finally, the behavior of such slabs is examined through a parametric study. The sensitivity of the material model to different material properties and edge restraints is also documented in the parametric study.