Title: Standard Specification for Plain Concrete Parking Lots (ACI 330.1)

Author(s): ACI Committee 330

Publication: Materials Journal

Volume: 90

Issue: 4

Appears on pages(s): 370-375

Keywords: concrete parking lots; concrete pavements; construction; curing; jointing; pavement; specification; texturing; Materials Research

DOI: 10.14359/3898

Date: 7/1/1993

Abstract:
This standard covers minimum requirements for the construction of plain concrete parking lots on grade. Included are requirements for materials, placing, texturing, curing, jointing, and opening to traffic.