Properties of Silica Fume Concrete and Mortar

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Properties of Silica Fume Concrete and Mortar

Author(s): Ziad Bayasi and Jing Zhou

Publication: Materials Journal

Volume: 90

Issue: 4

Appears on pages(s): 349-356

Keywords: compressive strength; concretes; flexural strength; silica fume; mechanical properties; permeability; slump; Materials Research

DOI: 10.14359/3892

Date: 7/1/1993

Abstract:
Investigates various properties of silica fume concrete, such as slump, air content, compressive strength, flexural strength, permeability, and permeable void volume. The effect of silica fume replacement ratio of cement is described. Also, the effects of aggregate content and graduation, water-binder (cement + silica fume), and superplasticizer dosage rate are discussed. The results are important in drawing parallels of plain and silica fume concrete mix design procedures. In this experimental investigation, silica fume-binder ratio ranges from 0 to 0.40, water-binder ratio ranges from 0.41 to 0.47, aggregate-binder ratio ranges from 1.0 to 4.0, and superplasticizer-binder ratio ranges from 0.01 to 0.05.