Title: Re-Evaluating the Slump Test

Author(s): Martin Mitteleacher

Publication: Concrete International

Volume: 14

Issue: 10

Appears on pages(s): 53-56

Keywords: air entrainment; batching; compressive strength; slump test; water-reducing admixtures; General

DOI:

Date: 10/1/1992

Abstract:
The comfortable relationship between slump and expected concrete ingredients has become tenuous with the introduction of air-entraining and water-reducing admixtures. The use of the slump test as a predictor of concrete strength needs to be re-evaluated.