Reclamation of a Failing Parking Garage

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reclamation of a Failing Parking Garage

Author(s): Myles A. Murray

Publication: Concrete International

Volume: 14

Issue: 9

Appears on pages(s): 48-51

Keywords: abrasive blasting; columns (supports); cores; corrosion; parking facilities; polyethylene fibers; reinforcing steel; shotcrete; silica fume; two-way slabs; General

DOI:

Date: 9/1/1992

Abstract:
A heavily corroded parking garage constructed in 1967 was so badly delaminated in 1987 that, without repairs, structural failure was likely within 5 years. The reinforced concrete structure had been designed as a two-way slab with mats of reinforcing steel in the top and bottom. The slab is 12 in. (300 mm) thick with columns 32 ft (9.7 m) on center, each way. The individual slab systems are 128 ft (39 m) square. The original specifications called for 3000 psi (21,000 kPa) concrete with 5 percent entrained air.