Performance Characteristics of Traffic Deck Membranes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Performance Characteristics of Traffic Deck Membranes

Author(s): Frank Reagan

Publication: Concrete International

Volume: 14

Issue: 6

Appears on pages(s): 48-51

Keywords: abrasion resistance; adhesion; bridge decks; low temperature; modulus of elasticity; permeability; reinforced concrete; tensile strength; safety; vapor barriers; waterproofing; General

DOI:

Date: 6/1/1992

Abstract:
Outlines factors to be considered when choosing membrane systems for traffic-bearing concrete structures. Some of these are permeability, adhesion, elongation, tensile strength, tear strength, modulus of elasticity, abrasion resistance, low-temperature flexibility, and safety.